Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styrolution® PS ECO 168N BC100 - PS - INEOS Styrolution

Material Data Center offers the following functions for Styrolution® PS ECO 168N BC100:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Styrolution PS datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 1.5 cm³/10min ISO 1133
Temperatura 200 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3300 MPa ISO 527
Carico unitario a trazione 59 MPa ISO 527
Deformazione a rottura 3 % ISO 527
Modulo a flessione, 23°C 2280 MPa ISO 178
Resistenza alla flessione 160 MPa ISO 178
Modulo di scorrimento a trazione, 1h 3300 MPa ISO 899-1
Modulo di scorrimento a trazione, 1000h 2600 MPa ISO 899-1
Ball indentation hardness 150 MPa ISO 2039-1
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 86[ann.] °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 98[ann.] °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 101 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 80 E-6/K ISO 11359-1/-2
ASTM Data
Temp.di rammollimento Vicat 108 °C ASTM D 1525
Other Standards[S]
Conduttività termica, stato solido 0.17 W/(m K) DIN 52612-1
S: These properties are reported by the producer according standards that are different to our defaults.  ann.: annealed
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 2.5 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 0.9 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 0.5 E-4 IEC 62631-2-1
Resistività volumica 1E16 Ohm*m IEC 62631-3-1
Resistività superficiale 1E14 Ohm IEC 62631-3-2
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 2 % ASTM D 1003
Trasmissione luminosa 89 % ASTM D 1003
Other Standards[S]
Indice di rifrazione 1.57 - ISO 489
S: These properties are reported by the producer according standards that are different to our defaults.
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1040 kg/m³ ISO 1183
Preparazione ProvetteValoreUnitáNorma del test
ISO Data
Stamp. ad Iniezione, temperatura dello stampo 40 °C ISO 294
Stamp. ad Iniezione, Velocità media d'iniezione 200 mm/s ISO 294
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Temperatura di fusione 180 - 280 °C -
Temperatura dello stampo 10 - 60 °C -
Raccomandazione de Processabilità EstrusioneValoreUnitáNorma del test
Type of extrusion sheet - -
Temperatura di fusione 250 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione di Lastre/Fogli
Forma fisica disponibile
Pellet
Caratteristiche speciali
Stabilizzato o stabile al calore
Caratteristiche
Miscela di resina, Schiumabile
Certifications
Contiene risorse rinnovabili, Contatto con gli alimenti, ISCC Plus
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.